ChemNet > Gold Suppliers > oceanchemical >

TPE-OW50 elastomer

TPE-OW50 elastomer

Category :

Catalyst and Auxiliary

CAS NO :
EC NO :
Molecular Formula :
Main Specifications :
Synonyms :
TPE-OW50 elastomer
Product description:
Outdoors using Cold-resistance (-50), Oil-resistance TPE elastomer cable and sheath materials (below that is simpled as TPE-OW50) is a body mixed by the special rubber and many kinds of plastics. and it is also researched and developed by Weifang Tianrui Chemical Co., Ltd. The development of TPE-OW50 elastomer mainly makes up the shortages of the general TPE elastomer. And it develops the broad  foreground for the general TPE.
 
Properties:
1. TPE-OW50 not only has good workability and the mechanical physical performance .
2. TPE-OW50 remarkably bears the ultraviolet radiation. After 720 hours ultraviolet radiation , its mechanical physical performance remains nearly the same as before .It can conform to the UL105 electric wire standard hot air circulation to get older (136*168).
3. TPE-OW50 has good oil-resistance. After dipping in Oil IRM902 for 168 hours at the centigrade 60, the Rates of tensile strength retention changes and elongation retention changes are more than 80%.
4. The TPE-OW50 elastomer has high temperature resistance .So in 150 temperature, under 2000g loads, the thermal deformation maintains in 50%. When Shore A equals78, its tensile strength can over 1400psi, and the tensile stretch is more than 300%.
5. TPE-OW50 elastomer has good flame- resistance . In ULSJE14AWG 16AWG AND 18AWG wires all pass FT2 VW-1 grades .
 
TPE-OW50 Physical and Mechanical Properties:
Properties
Isolation
Jacketing
Shore A (5 seconds)
80
78
Tensile Strength psi ≥
1300
1400
Tensile Stretch   %    ≥
300
330
Volume Resistivity (20℃) Ω.M≥
1.0*10 11
1.0*10 11
Voltage Break MV/M≥
25
25
Thermal Deformation 150℃ %
40
45
Cryogence property
 
 
Low Temperature Bending 4 hours/-50℃
Pass
Pass
Low Temperature Impact     -30℃
Pass
Pass
Infusing in Oil 1RM902 for 168 Hours /60℃
 
 
Tensile strength retention rate changes % ≥
80
80
 Elongation retention rate changes% ≥
80
80
Heat Aging 7 days /136℃
 
 
Tensile strength retention rate changes% ≥
80
80
 Elongation retention rate changes% ≥
80
80
Flame Resistance UL94V-0    mm
1
1
 
The ranges of usage:
TPE-OW50 are mainly used in the wires such as ULSJE 14AWG 16AWG 18AWG.At 50 after four hours of low temperature spooling, on the superficial have non dehiscence phenomenon and the wires also maintained certain flexibility.
Send your inquiry to TPE-OW50 elastomer supplier

Enter between 20 to 3,000 characters,English only.

Contact us
Company:
   Shandong Brother Sci.&Tech. Co.,Ltd
Contact:
   Bill Ju
Phone:
+86-536-5268256
Mobile phone:
+86-13863645520
Fax:
+86-536-5268259
E-mail:
Contact Supplier
Website:
http://www.oceanchemical.com
Address:
Shouguang Bohai Industry Zone ,Shandong ,China
Zip Code:
262714
World Wide ChemNet: - International - China - Korea
About Us - Top Products- Partner with Us - Contact Us - Help - Sitemap
ChemNet is a registered trademark of Zhejiang NetSun Co., Ltd.