Outdoors using Cold-resistance (-50), Oil-resistance TPE elastomer cable and sheath materials (below that is simpled as TPE-OW50) is a body mixed by the special rubber and many kinds of plastics. and it is also researched and developed by Weifang Tianrui Chemical Co., Ltd. The development of TPE-OW50 elastomer mainly makes up the shortages of the general TPE elastomer. And it develops the broad  foreground for the general TPE.
 
Properties:
1. TPE-OW50 not only has good workability and the mechanical physical performance .
2. TPE-OW50 remarkably bears the ultraviolet radiation. After 720 hours ultraviolet radiation , its mechanical physical performance remains nearly the same as before .It can conform to the UL105 electric wire standard hot air circulation to get older (136*168).
3. TPE-OW50 has good oil-resistance. After dipping in Oil IRM902 for 168 hours at the centigrade 60, the Rates of tensile strength retention changes and elongation retention changes are more than 80%.
4. The TPE-OW50 elastomer has high temperature resistance .So in 150 temperature, under 2000g loads, the thermal deformation maintains in 50%. When Shore A equals78, its tensile strength can over 1400psi, and the tensile stretch is more than 300%.
5. TPE-OW50 elastomer has good flame- resistance . In ULSJE14AWG 16AWG AND 18AWG wires all pass FT2 VW-1 grades .
 
TPE-OW50 Physical and Mechanical Properties:
Properties
Isolation
Jacketing
Shore A (5 seconds)
80
78
Tensile Strength psi ≥
1300
1400
Tensile Stretch   %    ≥
300
330
Volume Resistivity (20℃) Ω.M≥
1.0*10 11
1.0*10 11
Voltage Break MV/M≥
25
25
Thermal Deformation 150℃ %
40
45
Cryogence property
 
 
Low Temperature Bending 4 hours/-50℃
Pass
Pass
Low Temperature Impact     -30℃
Pass
Pass
Infusing in Oil 1RM902 for 168 Hours /60℃
 
 
Tensile strength retention rate changes % ≥
80
80
 Elongation retention rate changes% ≥
80
80
Heat Aging 7 days /136℃
 
 
Tensile strength retention rate changes% ≥
80
80
 Elongation retention rate changes% ≥
80
80
Flame Resistance UL94V-0    mm
1
1
 
The ranges of usage:
TPE-OW50 are mainly used in the wires such as ULSJE 14AWG 16AWG 18AWG.At 50 after four hours of low temperature spooling, on the superficial have non dehiscence phenomenon and the wires also maintained certain flexibility.


  Company: Shandong Brother Sci.&Tech. Co.,Ltd     [ China ]        
  Contact: Bill Ju
  Tel: +86-536-5268256
  Fax: +86-536-5268259
  Email: ocean@oceanchemical.com
Disclaimer statement:The information and data included above have been realized by the enterprises and compiled by the staff, and are subject to change without notice to you. The Chemnet makes no warranties or representations whatsoever regarding the facticity, accuracy and validity of such information and data. In order to ensure your interest, we suggest you chose the products posted by our gold suppliers or VIP members.