    Cas No. :39100000 Quantity: 200Kilograms
    Specs:620
    Price:9 USD Kilograms
    Payment Method: L/C,T/T
    RTV-2 liquid manual molding silicone rubber

    Brief description of RTV-2 liquid manual molding silicone rubber
    RTV-2 liquid manual molding silicone rubber is a flowable liquid, and the quality has nothing to do with the color. It consists of two components. Part A is a flowable liquid silicone rubber, part B is the curing agent. Firstly, after dealing with the original model, take some liquid silicone rubber , add 2%-3% curing agent of the amount of silicon, and mix them evenly. Then after vacuum-pumping the mixture, you can pour it into the mold frame. The silicone mold will cured in 2-3 hours.
    Note: The time for vacuum-pumping should be less than 3-5 mins ,otherwise, once the silicone rubber has cross-link reaction during vacuumizing, it will not be operated.

    Applications of RTV-2 liquid manual molding silicone rubber
    RTV-2 liquid manual molding silicone rubber is mainly used for model design of manual mold, PVC plastic molds, cement products, low melting point alloy molds, electronics, handicrafts, large-scale sculpture, reproduction of cultural relic, sole molds, pad printing allocation, Electronic equipment antivibration, etc.

    Brief features:
    1.Good elasticity
    2. Non deformation
    3. Heat resistance
    4. Low shrinkage.

    Operation Instruction:
    1)Correct mixing ratio
    2)Preparation of the Original molds
    3) Vacuum-Pumping Process

    Frequently asked questions of RTV-2 liquid manual molding silicon Rubber
    1. How to deal with the bubbles during the mixing process?
    It depends on your practical situation. Firstly you can deal the mixture with a vacuum machine if you have one; If no such machine, you can reduce the mixing ratio of the hardener from 4% to 1%-2%.Then in the prior period of the reaction of the mixture will be slower, then the air in the mixture will exhaust by itself for a longer curing time to release the bubble.

    Any more questions please feel free to contact Aimee:
    EMail:hysz(at)szrl(dot)net
    Mob:86-18938867541
  • CAS Registry Number:

    39100000
  • Company:

    Shenzhen Hong Ye Jie Technology Co., Ltd     [ China ]        
  • Contact:

    aimee
  • Tel:

    8675589948019
  • Fax:

    8675589948030
  • Email:

    hysz@szrl.net
Inquiry
Home Suppliers Product CAS Gmall